Nye Lubricants UniFlor 8531 (834-1) (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8531 (834-1) (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 178
178
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 230 cSt
230 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 31 cSt
31 cSt
Base Oil; ASTM D445
Evaporation Loss 0.00 %
0.00 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 257
257
ASTM D217
Penetration P(60), 1/10 mm 274
274
ASTM D217
Oil Separation 5.8 %
5.8 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -41.0 °C
-41.8 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(blnd)
Gellant Type PTFE