Material Notes:
Molecular Formula: C30H58O4SCas No.: 123-28-4Characteristics and Uses: As a thioester auxiliary antioxidant with good performance, it is namely applied to polyethylene, polypropylene, PVC, AS resin, ABS resin etc. It has excellent compatibility with Antioxidants 1010, 1076 etc.Storing and Packing: This product is nontoxic, inflammable, noncorrodible and well stable, packed in cardboard pails lined with plastic bags with the next capacity of 25 kg per bag.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 39.0 - 41.0 °C
102 - 106 °F
Optical Properties Metric English Comments
Transmission, Visible >= 97 %

@Wavelength 425 nm
>= 97 %

@Wavelength 425 nm
10g/100ml Toluene
>= 97 %

@Wavelength 500 nm
>= 97 %

@Wavelength 500 nm
10g/100ml Toluene
Descriptive Properties Value Comments
Appearance White flaky crystal
CAS Number 123-28-4
Chemical Name Dilauryl Thiodipropionate
Content (%) >99.0
Molecular Formula C30H58O4S
Solubility 10g dissolved in 100g solution
clarified at room temperature