Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omya OMYACARB® 520 - FL Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Omya North America
Trade Name OMYACARB®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omya OMYACARB® 520 - FL Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A high purity, fine, wet ground natural calcium carbonate surface-treated and activated for low humidity content.Applications: Adhesive applications where low moisture content and pick up is required.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Brightness 93.5 %
93.5 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.030 %
0.030 %
Moisture Loss at 110°C % (dry)
Particle Size 2.0 µm
2.0 µm
Median Diameter
Specific Surface Area 3.3 m²/g
3.3 m²/g
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Magnesium Carbonate % 1
Retained in 325 mesh (dry) ppm 1
Treatment % 0.8