Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Orion Engineered Carbons PUREX® HS 25 Carbon Black

Category Carbon , Carbon Black
Manufacturer Orion Engineered Carbons
Trade Name PUREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Orion Engineered Carbons PUREX® HS 25 Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.
Physical Properties Metric English Comments
Bulk Density 0.375 g/cc
0.0135 lb/in³
Pour Density; ASTM D 1513
Oil Absorption 83 %
83 %
(ml/100 g); Compressed Sample; ASTM D 3493
123 %
123 %
(ml/100 g); ASTM D 2414
Loss On Ignition <= 0.50 %
<= 0.50 %
Heating Loss; ASTM D 1509
Specific Surface Area 28 m²/g
28 m²/g
Statistical thickness surface area; ASTM D 6556
Iodine Absorption Number 28
28
mg/g; ASTM D 1510
Descriptive Properties Value Comments
Fines < 7.0 %
ASTM D 1508
Individual Pellet Hardness < 40 g
ASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue < 50 ppm
ASTM D 1514