Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers 10GF 10% Glass Fiber Reinforced ABS, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 10GF 10% Glass Fiber Reinforced ABS, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
10% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Filler Content 10 %
10 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
ASTM D648