| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) |
| Manufacturer | Pearl Engineering Polymers Limited |
| Trade Name | PEPLPET |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Pearl Engineering PEPLPET FR-101-H Monofilament Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | PEPL-10-W-21 |
| Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | PEPL-10-W-67 |
| Bead Size | 2.80 mm | 0.110 in | chip size, length; PEPL-10-W-71 |
| 3.10 mm | 0.122 in | chip size, D2; PEPL-10-W-71 | |
| 3.80 mm | 0.150 in | chip size, D1; PEPL-10-W-71 | |
| Viscosity Measurement | 0.70 - 0.74 | 0.70 - 0.74 | intrinsic, [dl/gm]; QCD--W1-42 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | <= 65.0 J/g | <= 28.0 BTU/lb | |
| Specific Heat Capacity | 1.10 J/g-°C @Temperature 20.0 °C |
0.263 BTU/lb-°F @Temperature 68.0 °F |
|
| 1.37 J/g-°C @Temperature 80.0 °C |
0.327 BTU/lb-°F @Temperature 176 °F |
||
| 1.44 J/g-°C @Temperature 100 °C |
0.344 BTU/lb-°F @Temperature 212 °F |
||
| 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
||
| 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
||
| Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
| 0.242 W/m-K @Temperature 20.0 °C |
1.68 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
solid | |
| Melting Point | 250 - 256 °C | 482 - 493 °F | QCD--W1-49 |
| Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
| Flash Point | 480 °C | 896 °F | |
| Oxygen Index | >= 30 % | >= 30 % | ASTM D 2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.20 % | <= 0.20 % | when packed; QCD--W1-54 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Acetaldehydes (ppm) | <1 | QCD--W1-53 |
| Chips per Gram | 30-36 | QCD--W1-47 |
| COOH end groups (mval/kg) | <25 | QCD--W1-43 |
| Fines (ppm) | <100 | QCD--W156 |