| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
| Melt Flow | 12 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
12 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 27.2 MPa | 3950 psi | (2 in/min); ASTM D638 |
| Elongation at Yield | 14 % | 14 % | ASTM D638 |
| Flexural Modulus | 1.00 GPa | 145 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
| Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | Method A; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | Unannealed; ASTM D648 |