Polimeri Europa Europrene® 1500 Emulsion Styrene-Butadiene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® 1500 Emulsion Styrene-Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Europrene® 1500 is an emulsion styrene-butadiene rubber obtained by cold polymerization using a rosin acid soap as emulsifier. A non-staining antioxidant is added during the production process.Key Features: E-SBR is a general purpose rubber characterized by good processability, mechanical properties and abrasion resistance. It has limited resistance to oil and weather but properly compounded, it is suitable for use in outdoor applications. The use of rosin acid soap results in a higher tack of the green compound and a slightly slower cure rate compared to fatty/rosin acid emulsified types.Main Applications: Tire manufacturing and retreading, conveyor belts, hoses and other mechanical goods.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Mooney Viscosity 52

@Temperature 100 °C
52

@Temperature 212 °F
ASTM D1646
Ash <= 0.50 %
<= 0.50 %
ASTM D5667
Chemical Properties Metric English Comments
Styrene Content 23.5 %
23.5 %
Bound; ASTM D5775
Descriptive Properties Value Comments
Organic Acid 6% wt
ASTM D5774
Soap < 0.3% wt
Users viewing this material also viewed the following: