Polimeri Europa Europrene Latice® 2430 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene Latice®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene Latice® 2430 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Europrene Latice® 2430 is an aqueous dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant.Key Features: The vulcanized latex shows excellent mechanical properties. Europrene Latice® 2430 can be blended with natural latex.Main Applications: Europrene Latice® 2430 is used for high stiffness molded foams. It can be used for gel and no-gel carpet foams.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Solids Content 68 %
68 %
Total; ASTM D1417
pH 10.5
10.5
ASTM D1417
Brookfield Viscosity 1100 cP
1100 cP
20 rpm; ASTM D1417
Chemical Properties Metric English Comments
Styrene Content 35 %
35 %
Bound; ASTM D5775