| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 84 | 84 | ASTM D2240 |
| Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.92 GPa | 424 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 79.4 MPa | 11500 psi | ASTM D790 |
| Flexural Modulus | 3.01 GPa | 437 ksi | ASTM D790 |
| Izod Impact, Notched | 13.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
24.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
| Dart Drop Total Energy | 71.2 J/cm @Temperature 23.0 °C |
0.133 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 133 J/cm @Temperature 23.0 °C |
0.249 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 61.0 µm/m-°C | 33.9 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 74.8 °C | 167 °F | conditioned @ 50 deg.C; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Flammability, UL94 | HB @Thickness 0.370 mm |
HB @Thickness 0.0146 in |
white; UL 94 |
| V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
All Color; UL 94 | |
| 5VA @Thickness 2.00 mm |
5VA @Thickness 0.0787 in |
white; UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.70e+15 ohm-cm @Thickness 1.22 mm |
7.70e+15 ohm-cm @Thickness 0.0480 in |
ASTM D257 |
| Surface Resistance | 4.70e+14 ohm @Thickness 1.22 mm |
4.70e+14 ohm @Thickness 0.0480 in |
ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 193 - 210 °C | 379 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Good Thermal Stability | |
| High Impact Resistance | ||
| Forms | Powder | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Outdoor Suitability | f1 | UL 746C |
| Processing Method | Extrusion | |
| Profile Extrusion | ||
| Sheet Extrusion | ||
| PVC Cell Classification | 1-42434-33-0100 | ASTM D4216 |
| 16354 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Fencing & Decking | |
| Film | ||
| Outdoor Applications | ||
| Profiles | ||
| Sheet |