| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible B5D05 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 58 | 58 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 20.5 MPa | 2970 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 17.4 MPa @Strain 100 % |
2520 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 310 % | 310 % | 51 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -11.0 °C | 12.2 °F | ASTM D746 |
| Oxygen Index | 26 % | 26 % | ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
| 196 - 207 °C | 385 - 405 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Features | General Purpose | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Consumer Applications | |
| Furniture | ||
| General Purpose |