| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible B87FB Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 80 | 80 | 15 sec; ASTM D2240 |
| 87 | 87 | ASTM D2240 | |
| Tensile Strength at Break | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 300 % | 300 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -30.0 °C | -22.0 °F | ASTM D746 |
| Oxygen Index | 25 % @Thickness 3.18 mm |
25 % @Thickness 0.125 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
| 191 - 202 °C | 376 - 396 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Features | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Sheet Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |