| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible XV 3704 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 84 | 84 | 15 sec; ASTM D2240 |
| 92 | 92 | ASTM D2240 | |
| Tensile Strength at Break | 19.4 MPa | 2810 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 12.3 MPa @Strain 100 % |
1780 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 340 % | 340 % | 510 mm/min; ASTM D638 |
| Compression Set | 45 % @Temperature 23.0 °C, Time 79200 sec |
45 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.607 GPa | 88.0 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -30.0 °C |
45.0 ksi @Temperature -22.0 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -36.7 °C | -34.1 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
| 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Features | Good Surface Finish | |
| Low Temperature Resistant | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Coextrusion | |
| Extrusion | ||
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Hose | |
| Seals | ||
| Tubing | ||
| Weatherstripping |