| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
| Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 105 | 105 | ASTM D785 |
| Hardness, Shore D | 79 | 79 | ASTM D2240 |
| Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.39 GPa | 347 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
| Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
| Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 81 % @Thickness 0.851 mm, Wavelength 400 nm |
81 % @Thickness 0.0335 in, Wavelength 400 nm |
Internal Method |
| 86.5 % @Thickness 0.851 mm, Wavelength 700 nm |
86.5 % @Thickness 0.0335 in, Wavelength 700 nm |
Internal Method |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 202 - 213 °C | 396 - 415 °F | Blow Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | FDA Food Contact, Unspecified Rating | |
| Appearance | Clear/Transparent | |
| Features | Food Contact Acceptable | |
| High Gloss | ||
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Bottles | |