| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 81 | 81 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 53.2 MPa | 7720 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.88 GPa | 418 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
| Flexural Modulus | 3.03 GPa | 439 ksi | ASTM D790 |
| Izod Impact, Notched | 0.410 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.768 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
| Dart Drop Total Energy | 85.4 J/cm @Temperature 23.0 °C |
0.160 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 85.4 J/cm @Temperature 23.0 °C |
0.160 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 79.1 °C | 174 °F | Annealed; ASTM D648 |
| 79.8 °C @Thickness 3.18 mm |
176 °F @Thickness 0.125 in |
Unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 76.6 °C | 170 °F | Annealed; ASTM D648 |
| 73.3 °C @Thickness 3.18 mm |
164 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 60 % | 60 % | 60°; ASTM D2457 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Cube | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Coextrusion | |
| Profile Extrusion | ||
| PVC Cell Classification | 12454 | ASTM D1784 |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Capstock | |
| Fencing & Decking | ||
| Outdoor Applications | ||
| Profiles |