| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable W2403 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 38 | 38 | 15 sec; ASTM D2240 |
| 50 | 50 | ASTM D2240 | |
| Tensile Strength at Break | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 280 % | 280 % | Type IV, 510 mm/min; ASTM D638 |
| Tensile Modulus | 0.0121 GPa | 1.75 ksi | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
| Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
| Oxygen Index | 24 % <br>@Thickness 1.91 mm |
24 % <br>@Thickness 0.0752 in |
ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 185 - 191 °C | 365 - 376 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Features | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Cable Jacketing | |
| Communication Wire Jacketing | ||
| Wire & Cable Applications |