| Category | Polymer , Thermoplastic , Polyurethane, TP |
| Manufacturer | PolyOne Corporation |
| Trade Name | Gravi-Tech™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Gravi-Tech™ GRV-UR-080-W Polyurethane, Unspecified (PUR, Unspecified).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 7.98 g/cc | 7.98 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 10.3 MPa | 1490 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 70 % | 70 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 0.00951 GPa | 1.38 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Modulus | 0.0896 GPa | 13.0 ksi | ASTM D790 |
| Izod Impact, Notched | 1.60 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 204 °C | 360 - 399 °F | |
| Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
| Drying Temperature | 65.6 °C | 150 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | High Density | |
| Non-Toxic | ||
| Forms | Pellets | |
| Generic Material | PUR, Unspecified | |
| Generic Name | Polyurethane, Unspecified (PUR, Unspecified) | |
| Processing Method | Injection Molding | |
| Regional Availability | Asia Pacific | |
| Uses | Industrial Applications | |
| Medical/Healthcare Applications | ||
| Projectiles | ||
| Sporting Goods | ||
| Weighting & Balancing |