| Category | Polymer , Thermoplastic , Nylon , Nylon 610 |
| Manufacturer | PolyOne Corporation |
| Trade Name | LubriOne™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne LubriOne™ NI-20GF/15T FR Polyamide 610 (Nylon 610).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 103 MPa | 14900 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 165 MPa | 23900 psi | ASTM D790 |
| Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
| Izod Impact, Notched | 0.930 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.74 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-0 | V-0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Flame Retardant | |
| Lubricated | ||
| Forms | Pellets | |
| Generic Material | Nylon 610 | |
| Generic Name | Polyamide 610 (Nylon 610) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Appliance Components | |
| Conveyor Parts | ||
| Printer Parts |