Material Notes:
Description/Features:High Performance Thermoplastic ElastomerWeatherable GradeApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Extrusion and MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Linear Mold Shrinkage 0.0103 cm/cm
0.0103 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 31
31
10 Sec; ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
9.65 MPa

@Strain 300 %
1400 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 550 %
550 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 75.4 kN/m
430 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 32 %
32 %
Method B, 73°F(23°C), 22 hrs; ASTM D395