Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 8.0
8.0
Instant; ASTM D2240
Tensile Strength, Yield 1.24 MPa
180 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
0.207 MPa

@Strain 300 %
30.0 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 1000 %
1000 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 5.78 kN/m
33.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 22 %
22 %
Method B, 73°F(23°C), 22 hrs; ASTM D395