Potters Industries Conduct-O-Fil® S3000-S2M Silver-Coated Solid Glass Spheres

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Conduct-O-Fil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Conduct-O-Fil® S3000-S2M Silver-Coated Solid Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-axis conductive films. Features good conductivity, low density compared to metal filler, spherical shape gives good flow in injection molding, light color.Information provided by Potters Industries.
Physical Properties Metric English Comments
Particle Size 41 µm
41 µm
Average Diameter
Component Elements Properties Metric English Comments
Silver, Ag 8.0 %
8.0 %
by weight