Proto3000 Objet Digital Materials™ DM_9870/9770 Rubber-like Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Objet Digital Materials™ DM_9870/9770 Rubber-like Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 75
65 - 75
ASTM D2240
Tensile Strength at Break 2.00 - 4.00 MPa
290 - 580 psi
ASTM D412
Elongation at Break 50 - 70 %
50 - 70 %
ASTM D638-05
Tear Strength 11.8 - 13.7 kN/m
67.2 - 78.4 pli
ASTM D624