Pyrotek M-8 Fiberseal Blanket

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek M-8 Fiberseal Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Stitched with high-temperature fibers. Contains no binders. Not changed by exposure to high temperatures.Dimensions610 mm x 7.6 m25 mm thickApplicationsHigh-temperature gaskets Furnace linings General insulation applications Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.128 g/cc
0.00462 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1427 °C
2601 °F