Pyrotek S-2 Fabric

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek S-2 Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Coarse fabric with low air permeability. Excellent mechanical strength and abrasion resistance.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.373 g/cc
0.0135 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 315 °C
599 °F