| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Durapro® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
| Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | ASTM D 570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 67 | 67 | ASTM D2240 |
| Tensile Strength | 32.4 MPa | 4700 psi | ASTM D638 |
| Elongation at Break | 200 % | 200 % | ASTM D638 |
| Tensile Modulus | 0.565 GPa | 82.0 ksi | ASTM D638 |
| Flexural Strength | 23.4 MPa | 3400 psi | ASTM D790 |
| Flexural Modulus | 0.607 GPa | 88.0 ksi | ASTM D790 |
| Compressive Strength | 19.3 MPa | 2800 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 0.452 GPa | 65.5 ksi | ASTM D695 |
| Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
| Izod Impact, Notched | 18.69 J/cm | 35.00 ft-lb/in | ASTM D256 |
| Coefficient of Friction, Dynamic | 0.080 | 0.080 | dry vs. steel; QTM55007 |
| Sand Slurry | 15 | 15 | 1018 steel = 100; ASTM D4020 |
| Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
| Abrasion | 130 | 130 | Sand Wheel; TIVAR® 1000 = 100; ASTM G-65 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 234 µm/m-°C @Temperature -40.0 - 150 °C |
130 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
| Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 3.17 mm |
HB @Thickness 0.125 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | 1e+13 - 1e+15 ohm | 1e+13 - 1e+15 ohm | EOS/ESD S11.11 |
| Dielectric Constant | 2.3 @Frequency 1.00e+6 Hz |
2.3 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dissipation Factor | <= 0.00050 @Frequency 1.00e+6 Hz |
<= 0.00050 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Unacceptable | Unacceptable | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |