| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Sanalite® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
| Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | ASTM D2240 |
| Tensile Strength | 31.7 MPa | 4600 psi | ASTM D638 |
| Elongation at Break | 400 % | 400 % | ASTM D638 |
| Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
| Flexural Strength | 31.7 MPa | 4600 psi | ASTM D790 |
| Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
| Compressive Strength | 31.7 MPa | 4600 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 0.689 GPa | 100 ksi | ASTM D695 |
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 110 µm/m-°C @Temperature -40.0 - 149 °C |
61.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Melting Point | 127 °C | 260 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | Yes | Yes | |
| FDA | Yes | Yes | |
| NSF | Yes | Yes | STD 2 & 51 |
| USDA | Yes | Yes | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Unacceptable | Unacceptable | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural | |
| Machinability | 3 | 1-10, 1=Easier to Machine |