| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
| Water Absorption | 0.11 % | 0.11 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 98 | 98 | ASTM D785 |
| Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 4.41 GPa | 640 ksi | ASTM D638 |
| Flexural Strength | 115.5 MPa | 16750 psi | ASTM D790 |
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
| Compressive Strength | 125 MPa | 18200 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 4.14 GPa | 600 ksi | ASTM D695 |
| Shear Strength | 77.9 MPa | 11300 psi | ASTM D732 |
| Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
| K (wear) Factor | >= 1010 x 10<sup>-8</sup> mm³/N-M | >= 500 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM55010 |
| Limiting Pressure Velocity | 0.0771 MPa-m/sec | 2200 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 45.0 µm/m-°C @Temperature -40.0 - 149 °C |
25.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM F433 |
| Melting Point | 340 °C | 644 °F | |
| Maximum Service Temperature, Air | 249 °C | 480 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 149 °C | 300 °F | ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
Crystalline; ASTM D3418 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | EOS/ESD S11.11 |
| Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
| Dielectric Constant | 4.13 @Frequency 1.00e+6 Hz |
4.13 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 14.8 kV/mm | 376 kV/in | ASTM D149 |
| Dissipation Factor | 0.0040 @Frequency 1e+6 Hz |
0.0040 @Frequency 1e+6 Hz |
ASTM D150 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Acceptable | Acceptable | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |