Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RVL36 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RVL36 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* VERTON* RVL36 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
5 mm/min; ISO 527
Elongation at Break 2.9 %
2.9 %
5 mm/min; ISO 527
Flexural Strength 258 MPa
37400 psi
2 mm/min; ISO 178
Flexural Modulus 8.30 GPa
1200 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 258 °C
496 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af