Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GA-509ORLT PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-509ORLT PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 71 - 80
71 - 80
ASTM D2240
Tensile Strength 13.1 MPa
1900 psi
ASTM D412
15.59 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2261 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
15.98 MPa

@Treatment Temp. 100 °C,
Time 346000 sec
2318 psi

@Treatment Temp. 212 °F,
Time 96.0 hour
Aging in ASTM Oil #2
Elongation at Break 325 %
325 %
ASTM D412
247 %

@Treatment Temp. 100 °C,
Time 346000 sec
247 %

@Treatment Temp. 212 °F,
Time 96.0 hour
Aging in ASTM Oil #2
276.25 %

@Treatment Temp. 136 °C,
Time 605000 sec
276.25 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
Thermal Properties Metric English Comments
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Oxygen Index 29 %
29 %
ASTM D2863
Users viewing this material also viewed the following: