Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufTech™ SE11-019D PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ SE11-019D PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Automotive – 90A PVC, integral colored, exterior weatherable, extrusion & injection molding compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 86.87 - 97.09

@Temperature 85.0 °C,
Time 605000 sec
86.87 - 97.09

@Temperature 185 °F,
Time 168 hour
Heat Aging; ISO 188, Method B
85.0 - 95.0

@Time 15.0 sec
85.0 - 95.0

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 17.0 MPa
2470 psi
500mm/min; ISO 527, 1A
18.0859 MPa

@Temperature 85.0 °C,
Time 605000 sec
2623.14 psi

@Temperature 185 °F,
Time 168 hour
Heat Aging; ISO 188, Method B
Elongation at Break 275 %
275 %
500mm/min; ISO 527, 1A
293.7 %

@Treatment Temp. 85.0 °C,
Time 605000 sec
293.7 %

@Treatment Temp. 185 °F,
Time 168 hour
Heat Aging; ISO 188, Method B
Descriptive Properties Value Comments
Cold Flex -34°C
SAE J323, Method A, No cracks
Users viewing this material also viewed the following: