Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1030 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarCLEAR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1030 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: StarCLEAR CLR-1030 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Features:Soft TouchRubbery FeelExcellent ColorabilityExcellent ClarityProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Viscosity 9400 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
9400 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 29

@Time 10.0 sec
29

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 5.93 MPa

@Time 7200 sec
860 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 715 %

@Time 7200 sec
715 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00145 GPa

@Time 7200 sec
0.210 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 11.0 kN/m
63.0 pli
ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear' but thickness not quantified
Descriptive Properties Value Comments
Color Clear