Material Notes:
Description: EC102 electrically-conductive silicone performs three distinct functions: the cabon filler in it allows it to act as a low amperage conductor; it shields RF and EM interference; and it protects against electrostatic discharge. All data based on a 0.02 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Yield 4.83 MPa
700 psi
ASTM D412
Elongation at Break 200 %
200 %
ASTM D412
Tear Strength 10.5 kN/m
60.0 pli
Initial Tear Strength; ASTM D624, Die B
Compression Set 20 %

@Temperature 100 °C
20 %

@Temperature 212 °F
Constant Deflection, Value given for 22 hr; ASTM D395
Electrical Properties Metric English Comments
Volume Resistivity 5.0 ohm-cm
5.0 ohm-cm
ASTM D991
Descriptive Properties Value Comments
Color Black