| Category | Ceramic , Carbide |
| Manufacturer | Sapco |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Sapco Si.SiC Silicon Carbide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.10 g/cc | 0.112 lb/in³ | |
| Open Porosity | 0.00 % | 0.00 % | |
| Weibull Modulus | 10 | 10 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Mohs | 9.0 | 9.0 | |
| Tensile Strength, Ultimate | 390 MPa | 56600 psi | |
| Modulus of Elasticity | 410 GPa | 59500 ksi | |
| Flexural Strength | 400 MPa | 58000 psi | |
| Compressive Strength | 2000 MPa | 290000 psi | |
| Poissons Ratio | 0.24 | 0.24 | |
| Shear Modulus | 165 GPa | 23900 ksi | Calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 4.30 µm/m-°C @Temperature 20.0 °C |
2.39 µin/in-°F @Temperature 68.0 °F |
|
| Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
| Thermal Conductivity | 160 W/m-K | 1110 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 1350 °C | 2460 °F |