Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone)

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Glass Filled
Manufacturer Sawbones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid-shaft area has an intermedullarly canal.Fourth-Generation Composite Bones Have Improved Properties Fourth-generation composite cortical bone has been developed in order to meet the demanding needs of in vitro experiments, fatigue testing and to more closely simulate natural cortical bone. The result is a composite bone with enhancements to the following properties: Fracture Toughness - Fatigue Crack Resistance Fatigue Life - Implant Subsidence Tensile Strength & Modulus - Compressive Strength & Modulus Thermal Stability - Moisture Resistance No changes have been made to the anatomical structure of the bones.Information provided by Sawbones.
Physical Properties Metric English Comments
Density 0.270 g/cc
0.00975 lb/in³
Solid
0.320 g/cc
0.0116 lb/in³
Cellular
Mechanical Properties Metric English Comments
Compressive Strength 5.40 MPa
783 psi
Cellular; ASTM D1621
6.00 MPa
870 psi
Solid; ASTM D1621
Compressive Modulus 0.137 GPa
19.9 ksi
Cellular; ASTM D1621
0.155 GPa
22.5 ksi
Solid; ASTM D1621
Poissons Ratio 0.30
0.30
ASTM D1621