| Category | Ceramic , Glass |
| Manufacturer | Schott North America |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott FIOLAX® clear Neutral Glass Tubing.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.34 g/cc @Temperature 25.0 °C |
0.0845 lb/in³ @Temperature 77.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 300 °C |
2.72 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
| Transformation Temperature, Tg | 565 °C | 1050 °F | |
| 565 °C | 1050 °F | ||
| 785 °C | 1450 °F | ||
| 1160 °C | 2120 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 92 - 93 % @Wavelength 400 - 800 nm, Thickness 1.00 mm |
92 - 93 % @Wavelength 400 - 800 nm, Thickness 0.0394 in |
|
| IR Transmittance | 24 % @Thickness 1.00 mm, Wavelength 2800 nm |
24 % @Thickness 0.0394 in, Wavelength 2800 nm |
|
| <= 30 % @Wavelength >=3500 nm, Thickness 1.00 mm |
<= 30 % @Wavelength >=3500 nm, Thickness 0.0394 in |
||
| 60 % @Thickness 1.00 mm, Wavelength 3300 nm |
60 % @Thickness 0.0394 in, Wavelength 3300 nm |
||
| 90 - 93 % @Wavelength 800 - 2500 nm, Thickness 1.00 mm |
90 - 93 % @Wavelength 800 - 2500 nm, Thickness 0.0394 in |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 5.0 % | 5.0 % | |
| B2O3 | 10.5 % | 10.5 % | |
| CaO | 1.5 % | 1.5 % | |
| Na2O | 7.0 % | 7.0 % | |
| SiO2 | 75 % | 75 % |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 1 | 1 | DIN 12116 |
| Alkali Class, AR | 2 | 2 | ISO 695 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Glasses in Laboratory Apparatus | Type I, Class B | ASTM E 438 |
| Hydrolytic Resistance | Class HGB 1 | ISO 719 |
| fulfilled | JP | |
| Type I | Ph. Eur. | |
| Type I | USP |