Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott NEO 1730 Alkaline Earth Aluminosilicate Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name NEO
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Schott NEO 1730 Alkaline Earth Aluminosilicate Glass.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive, household, and general lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.67 g/cc
<br>@Temperature 25.0 °C
0.0965 lb/in³
<br>@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C
<br>@Temperature 20.0 - 300 °C
2.50 µin/in-°F
<br>@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 715 °C
1320 °F
ISO 7884-8
Softening Point 935 °C
1720 °F
Viscosity 10&lt;sup&gt;7.6&lt;/sup&gt; dPa s; ISO 7884-3
Working Point 1210 °C
2210 °F
Viscosity 10&lt;sup&gt;4&lt;/sup&gt; dPa s; ISO 7884-2
Annealing Point 725 °C
1340 °F
Viscosity 10&lt;sup&gt;13&lt;/sup&gt; dPa s; ISO 7884-4
Strain Point 675 °C
1250 °F
Viscosity 10&lt;sup&gt;14.5&lt;/sup&gt; dPa s; ISO 7884-7
Optical Properties Metric English Comments
Refractive Index 1.548
<br>@Wavelength 587.6 nm
1.548
<br>@Wavelength 587.6 nm
Transmission, Visible 37 %
<br>@Thickness 1.00 mm,<br> Wavelength 585 nm
37 %
<br>@Thickness 0.0394 in,<br> Wavelength 585 nm
65 %
<br>@Thickness 1.00 mm,<br> Wavelength 750 nm
65 %
<br>@Thickness 0.0394 in,<br> Wavelength 750 nm
88 %
<br>@Thickness 1.00 mm,<br> Wavelength 775 nm
88 %
<br>@Thickness 0.0394 in,<br> Wavelength 775 nm
87 - 90 %
<br>@Wavelength 375 - 500 nm,<br> Thickness 1.00 mm
87 - 90 %
<br>@Wavelength 375 - 500 nm,<br> Thickness 0.0394 in
88 - 90 %
<br>@Wavelength 620 - 725 nm,<br> Thickness 1.00 mm
88 - 90 %
<br>@Wavelength 620 - 725 nm,<br> Thickness 0.0394 in
IR Transmittance 65 %
<br>@Thickness 1.00 mm,<br> Wavelength 800 nm
65 %
<br>@Thickness 0.0394 in,<br> Wavelength 800 nm
UV Transmittance 12 %
<br>@Thickness 1.00 mm,<br> Wavelength 300 nm
12 %
<br>@Thickness 0.0394 in,<br> Wavelength 300 nm
58 %
<br>@Thickness 1.00 mm,<br> Wavelength 330 nm
58 %
<br>@Thickness 0.0394 in,<br> Wavelength 330 nm
72 %
<br>@Thickness 1.00 mm,<br> Wavelength 340 nm
72 %
<br>@Thickness 0.0394 in,<br> Wavelength 340 nm
Component Elements Properties Metric English Comments
Alkalis <= 0.030 %
<= 0.030 %
Total Alkali Oxide
Chemical Properties Metric English Comments
Acid Class, SR 1
1
DIN 12116
Alkali Class, AR 2
2
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 1
ISO 719