Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott SF5 Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott SF5 Glass.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 4.07 g/cc
0.147 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 410
410
.1/20
Modulus of Elasticity 56.0 GPa
8120 ksi
Poissons Ratio 0.233
0.233
Shear Modulus 23.0 GPa
3340 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.56 µin/in-°F

@Temperature -22.0 - 158 °F
9.00 µm/m-°C

@Temperature 20.0 - 300 °C
5.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 425 °C
797 °F
Optical Properties Metric English Comments
Refractive Index 1.6727

@Wavelength 587.6 nm
1.6727

@Wavelength 587.6 nm
n<sub>d</sub>
1.67764

@Wavelength 546.1 nm
1.67764

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 95 %

@Thickness 10.0 mm,
Wavelength 380 nm
95 %

@Thickness 0.394 in,
Wavelength 380 nm
98.3 %

@Thickness 10.0 mm,
Wavelength 405 nm
98.3 %

@Thickness 0.394 in,
Wavelength 405 nm
99.5 %

@Thickness 10.0 mm,
Wavelength 460 nm
99.5 %

@Thickness 0.394 in,
Wavelength 460 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %

@Thickness 0.394 in,
Wavelength 580 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 84.7 %

@Thickness 10.0 mm,
Wavelength 2500 nm
84.7 %

@Thickness 0.394 in,
Wavelength 2500 nm
99.5 %

@Thickness 10.0 mm,
Wavelength 1530 nm
99.5 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 20 %

@Thickness 10.0 mm,
Wavelength 334 nm
20 %

@Thickness 0.394 in,
Wavelength 334 nm
62.6 %

@Thickness 10.0 mm,
Wavelength 350 nm
62.6 %

@Thickness 0.394 in,
Wavelength 350 nm
88.2 %

@Thickness 10.0 mm,
Wavelength 365 nm
88.2 %

@Thickness 0.394 in,
Wavelength 365 nm
91.5 %

@Thickness 10.0 mm,
Wavelength 370 nm
91.5 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 2.0
2.0
Alkali Class, AR 2.3
2.3
Stain Resistance Class, FR 1.0
1.0
Descriptive Properties Value Comments
B 1
Climatic Resistance Test CR 1
HG 2
K (10-6mm2/N) 2.28
Phosphate Resistance PR 3
T1013.0 (°C) 421
T107.6 (°C) 580