| Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber |
| Manufacturer | Seals Eastern, Inc |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Seals Eastern 5483 Nitrile Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D297, 15 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 70 | >= 70 | ASTM D2240, Type A |
| 80 | 80 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 6.909 MPa | >= 1002 psi | ASTM D412 Method A |
| 11.76 MPa | 1705 psi | AVG; ASTM D412 Method A | |
| 11.64 MPa @Temperature 100 °C, Time 252000 sec |
1688 psi @Temperature 212 °F, Time 70.0 hour |
ASTM D865 | |
| Tensile Strength, Yield | >= 0.538 MPa | >= 78.0 psi | Stress at Elongation M50; ASTM D412 Method A |
| >= 1.06 MPa | >= 154 psi | Stress at Elongation M100; ASTM D412 Method A | |
| 1.33 MPa | 193 psi | AVG Stress at Elongation M25; ASTM D412 Method A | |
| 2.15 MPa | 312 psi | AVG Stress at Elongation M50; ASTM D412 Method A | |
| 4.73 MPa | 686 psi | AVG Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 131 % | >= 131 % | ASTM D412 Method A |
| 242 % | 242 % | AVG; ASTM D412 Method A | |
| 273.5 % @Temperature 100 °C, Time 252000 sec |
273.5 % @Temperature 212 °F, Time 70.0 hour |
ASTM D865 | |
| Modulus of Elasticity | 0.007763 GPa | 1.126 ksi | ASTM D412 Method A |
| Shear Modulus | 0.00259 GPa | 0.375 ksi | ASTM D412 Method A |
| Secant Modulus | 0.007302 GPa | 1.059 ksi | ASTM D412 Method A |
| Compression Set | 13 % @Temperature 100 °C, Time 79200 sec |
13 % @Temperature 212 °F, Time 22.0 hour |
ASTM D395, Test B |
| 18 % @Temperature 100 °C, Time 252000 sec |
18 % @Temperature 212 °F, Time 70.0 hour |
ASTM D395, Test B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | -46.7 °C | -52.0 °F | ASTM D1329 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 60.0 Month | 60.0 Month | ASTM D395, Test B |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 20 |