Sekisui PIOCELAN LP-60E Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN LP-60E Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: General molding articles; Packing material for industrial parts; and Returnable containers for electronic parts.Information provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0167 g/cc
0.000603 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.2664 MPa
38.64 psi
ASTM D3575
Elongation at Break 9.4 %
9.4 %
ASTM D3575
Flexural Strength 0.1667 MPa
24.18 psi
ASTM D790
Flexural Modulus 0.008025 GPa
1.164 ksi
ASTM D790
Compressive Strength 0.1123 MPa

@Strain 25.0 %
16.29 psi

@Strain 25.0 %
ASTM D3575
0.1742 MPa

@Strain 50.0 %
25.26 psi

@Strain 50.0 %
ASTM D3575
0.3893 MPa

@Strain 75.0 %
56.46 psi

@Strain 75.0 %
ASTM D3575
Compression Set 38.1 %
38.1 %
ASTM D3575
Descriptive Properties Value Comments
Color White
Range of center value of pre-expanded particles 0.17-0.24 in