Shamrock Technologies NanoFLON® P 40A Thermoplastic Grade PTFE Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Shamrock Technologies
Trade Name NanoFLON® P
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shamrock Technologies NanoFLON® P 40A Thermoplastic Grade PTFE Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micron range (200 - 700 nanometers), as well as tightly-controlled chemical and physical properties. This significantly impacts molecular weight, crystallinity and morphology f the nanosized PTFE, thereby achieving key PTFE properties, including slip, refractive index, wettability surfactant and dielectric constant. NanoFlon P powder is agglomerated to 10 - 15 microns to minimize dusting during handling and is designed to disperse with regular mixing. the agglomerates break down with a resulting average particle size ranging from 200 - 700 nanometers. This provides up to one hundred times the surface area of other PTFE particles at equal weight (3µ vs. .3µ) for enhanced surface energy properties.Application:High intensity dispersion recommended, such as Medium mill or twin screw extruder processOffset, gravure and flexographic inksDigital and electronic inksCoatings: Industrial, automotive top coats, etc.Optical coatingsUV protectionFade resistanceThermoplastic fibersPlastic/Thermoplastic gears componentsWire and cableElastomeric seals and partsCosmetics, personal care products, hair care products and sunscreensLubricants, greases and oilsAgricultural chamicals and pesticidesTextile fibersElectronics/Electrical coatings and componenetsPolymeric computer chipsSpeciality: Food ContactInformation provided by Shamrock Technologies
Physical Properties Metric English Comments
Particle Size 0.20 - 0.70 µm
0.20 - 0.70 µm
Dispersed
200 - 500 µm
200 - 500 µm
Dry
Thermal Properties Metric English Comments
Melting Point 326 °C
619 °F
Descriptive Properties Value Comments
Appearance Free flowing powder
Color White