Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 002-2003Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.16 g/cc
2.13 - 2.16 g/cc
Bulk Density 0.400 - 0.600 g/cc
0.0145 - 0.0217 lb/in³
Particle Size 100 - 260 µm
100 - 260 µm
Mechanical Properties Metric English Comments
Tensile Strength >= 25.5 MPa
>= 3700 psi
Qualified
>= 27.0 MPa
>= 3920 psi
Grade A
Elongation at Break >= 250 %
>= 250 %
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 60.0 kV/mm
>= 1520 kV/in
Grade A
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
For Check Execute according to requirement of HG/T3028-1999
For Process Molding
Smoothness & Cleanliness Grade A: Clean and white surface, even texture, no foreign matters. D = 57mm, no color difference for rod color cross-section
Qualified: Clean and white surface, even texture, no metal residue, residue quantity (<1mm) < 2
Thermal Inst. Index <20