Shin-Etsu Silicones X-52-7073 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones X-52-7073 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
True
Volatiles 0.30 %
0.30 %
Particle Size 12 µm
12 µm
Mechanical Properties Metric English Comments
Hardness, Shore A 12
12
Rubber
Descriptive Properties Value Comments
Nature of Silicone Rubber Core Alkyl Dimethyl
Shape Sphere
Squalane 15
Swell (g/5g) 12
6cs
9
D5