Sibur PL-2PS Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur PL-2PS Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure.
Physical Properties Metric English Comments
Melt Index of Compound 8.0 g/10 min
8.0 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore A <= 65
<= 65
Tensile Strength at Break >= 7.84 MPa
>= 1140 psi
Elongation at Break >= 300 %
>= 300 %
Thermal Properties Metric English Comments
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 90 minutes