| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) |
| Manufacturer | Sichuan Deyang Chemical Co. Ltd. |
| Trade Name | Haton® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.55 g/cc | 0.0560 lb/in³ | GB/T 1033.1-2008 |
| Water Absorption | 0.020 % | 0.020 % | GB/T 1034-2008 |
| Linear Mold Shrinkage, Flow | 0.0026 cm/cm | 0.0026 in/in | GB/T 15585-1995 |
| Linear Mold Shrinkage, Transverse | 0.0078 cm/cm | 0.0078 in/in | GB/T 15585-1995 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 102 | 102 | GB/T 3398.2-2008 |
| Tensile Strength | 136 MPa | 19700 psi | GB/T 1040.2-2006 |
| Elongation at Break | 2.1 % | 2.1 % | GB/T1040.2-2006 |
| Flexural Strength | 218 MPa | 31600 psi | GB/T 9341-2008 |
| Flexural Modulus | 11.2 GPa | 1620 ksi | GB/T 9341-2008 |
| Izod Impact, Notched (ISO) | 17.2 kJ/m² | 8.18 ft-lb/in² | GB/T 1843-2008 |
| Izod Impact, Unnotched (ISO) | 58.0 kJ/m² | 27.6 ft-lb/in² | GB/T 1843-2008 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
| Deflection Temperature at 1.8 MPa (264 psi) | 262 °C | 504 °F | GB/T 1634.2-2004 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.30e+16 ohm-cm | 2.30e+16 ohm-cm | GB/T1410-2006 |
| Surface Resistivity per Square | 3.00e+15 ohm | 3.00e+15 ohm | GB/T1410-2006 |
| Dielectric Constant | 4.0 | 4.0 | GB/T 1409-2006 |
| Dielectric Strength | 16.0 kV/mm | 406 kV/in | GB/T1408.1-2006 |
| Dissipation Factor | 0.0020 | 0.0020 | GB/T 1409-2006 |