Material Notes:
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use in liquid colorant applications where processing temperatures are below the volatilization point of the carrier. Sparkle Silvex® C grades are compatible with a variety of resins including polyolefins and styrene. Sparkle Silvex® C grades are dampened with a pharmaceutical grade mineral oil and are suitable for applications which require FDA compliance. Specific FDA compliance information is available upon request. In order to maintain optimum aesthetics, Sparkle Silvex® grades should be dispersed properly.Applications: Plastics
Physical Properties Metric English Comments
Particle Size 16 µm
16 µm
Thermal Properties Metric English Comments
Flash Point 221 °C
430 °F
Descriptive Properties Value Comments
% Carrier 20
Carrier Mineral Oil