Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DIOFAN® A 050 is a standard PVDC latex grade for coatings on various substrates. It is generally used as a topcoat on paper, cardboard and as a coating on plastic films.Features: Moisture Barrier; Oxygen BarrierUses: Coating ApplicationsAdditional Properties: Density - 1.650 g/cm³; Density - 1.310 g/cm³; Emulsion Type - Anionic; Filmability - 18 °C; Heat Seal Maximum Resistance - 2.2 N/cm; Heat Seal Threshold - 110 °C; Oxygen Transmission Rate - ASTM D3985 54 cm³/m²/bar/24 hr; pH - 3.0; Shelf Life - (23°C): 12 month; Solids Content - 58 %; Surface Tension - 32 mN/m; Viscosity - (20°C): 10 mPa·sInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 16.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
1.03 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.21
0.21
vs. Itself; ASTM D1894
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid