Solvay Specialty Polymers Diofan® B 206 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® B 206 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Diofan® B 206 is a PVDC latex designed for high speed coating process of plastic films. This grade is recommended for food packaging applications when both good barrier properties and low sealing temperatures are needed.Features: Moisture Barrier; Oxygen BarrierUses: Barrier Coatings; Coating ApplicationsAdditional Properties: Density - 1.650 g/cm³; Density - 1.320 g/cm³; Emulsion Type - Anionic; Filmability - 13 °C; Heat Seal Maximum Resistance - 1.8 N/cm; Heat Seal Threshold - 104 °C; Oxygen Transmission Rate - ASTM D3985 35 cm³/m²/bar/24 hr; pH - 2.0; Shelf Life - (23°C): 12 month; Solids Content - 60 %; Surface Tension - 46 mN/mInformation provided by Solvay Specialty Polymers.
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.30
0.30
vs. Itself; ASTM D1894
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid