Solvay Specialty Polymers Tecnoflon® VPL 85730 / VPL 45730 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Tecnoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Tecnoflon® VPL 85730 / VPL 45730 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tecnoflon® VPL 85730 and VPL 45730 are very low temperature peroxide curable fluoroelastomers with outstanding low temperature flexibility (TR10 = -30°C). They show an improved chemical resistance if compared to Tecnoflon® PL grades with similar TR10. Like all other Tecnoflon® peroxide curable grades, they exhibit excellent processability; moreover they need very short post-curing cycles.Features: Fast Cure; Good Chemical Resistance; Good Flow; Good Mold Release; Good Processability; Low Temperature FlexibilityUses: Belts/Belt Repair; Blending; Gaskets; Hose; Low Temperature Applications; Profiles; Seals; SheetAdditional Properties: Fluorine Content - 67 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Mooney Viscosity 25 - 45

@Temperature 121 °C
25 - 45

@Temperature 250 °F
ML 1+10; ASTM D1646
Descriptive Properties Value Comments
Availability Europe; North America
Color Translucent
Form Slab
Processing Technique Calendering; Compounding
Compression Molding; Extrusion
Injection Molding; Resin Transfer Molding