| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 65 | 65 | ISO 868 |
| Tensile Strength at Break | 12.8 MPa | 1860 psi | ISO R 527 |
| Elongation at Break | 370 % | 370 % | ISO R 527 |
| Abrasion | 120 | 120 | Close, mm³; ISO 4649 |