Styron XZ 94445.00 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 94445.00 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Performance Features: Control of moisture vapor permeability, high water resistanceApplications: Waterproofing MembranesEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 51 %
51 %
pH 6.5
6.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 6.00 °C
42.8 °F